Sunday 6 February 2011

fragility samples

I experimented with home made glazes, Lithium white, Barium turqoise, tin white with cobalt oxide and green slip sprayed. The form split and cracked during the drying and firing process.


Screen print on to clay and then pressed into my plaster mould. Glazed with tin white.
I experimented with slip casting but pouring in glazes and coloured slip before the casting slip I then fired it straight to earthenware.

No comments:

Post a Comment